东洋纺TPE PELPRENE P40B物性表供应相关介绍如下:
Molding shrinkage of PELPRENE
3. Standard temperature for extrusion of PELPRENE
Brands | P30B? P40H | P55B? P90B S1001 | P150B? P280B S2001? S3001 | E450B S6001? S9001 |
---|---|---|---|---|
Cylinder temperature 1 | 160-170 | 190-200 | 200-220 | 220-230 |
2 | 180-190 | 200-220 | 220-230 | 230-240 |
3 | 180-190 | 200-220 | 220-230 | 230-240 |
4. Standard temperature for blow molding of PELPRENE (°C)
Brands | P46D | P55B-07 |
---|---|---|
Cylinder temperature 1 | 220-230 | 190-200 |
2 | 220-230 | 200-220 |
3 | 220-240 | 200-220 |
Mold temperature | 20-40 | 20-60 |
Molding shrinkage R90A:1.5% P55B-07:2%