PC基础创新塑料(南沙)HF1140-111 FDA 食品接触, 未评
: 本公司可以免费提供物性SGS MDS ROHS MSDS UL等证书产品说明 | |
Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with biocompatibility information and should not be used for medical applications which require biocompatibility. Alternative grade HP1. | |
总体 | |
材料状态 | 已商用:当前有效 |
资料 1 | Technical Datasheet |
UL 黄卡 2 | E121562-220945 |
搜索 UL 黄卡 | SABIC Innovative PlasticsLEXAN™ |
供货地区 | 北美洲 |
性能特点 | 尺寸稳定性良好耐热性,中等食品接触的合规性一次性中等透明度 |
机构评级 | FDA 食品接触, 未评级 |
加工方法 | 注射成型 |
多点数据 | Coefficient of Thermal Expansion vs. Temperature (ASTM E831)Elastic Modulus vs Temperature (ASTM D4065)Flexural DMA (ASTM D4065)Shear DMA (ASTM D4065)Specific Heat vs. Temperature (ASTM D3417)Tensile Creep (ASTM D2990)Tensile FatigueTensile Stress vs. Strain (ASTM D638)Thermal Conductivity vs. Temperature (ASTM E1530)Viscosity vs. Shear Rate (ASTM D3835) |
物理性能 | 额定值 | 单位制 | 测试方法 |
比重 | ASTM D792 | ||
-- | 1.20 | ||
-- | 1.19 | g/cm3 | |
特定体积 | 23.0 | in3/lb | ASTM D792 |
熔流率 (300°C/1.2 kg) | 25 | g/10 min | ASTM D1238 |
溶化体积流率(MVR) (300°C/1.2 kg) | 1.40 | in3/10min | ISO 1133 |
收缩率 - 流动 (0.126 in) | 0.0050 到 0.0070 | in/in | Internal Method |
吸水率 | ASTM D570 | ||
24 hr | 0.15 | % | |
平衡, 73°F | 0.35 | % | |
平衡, 212°F | 0.58 | % | |
硬度 | 额定值 | 单位制 | 测试方法 |
洛氏硬度 | ASTM D785 | ||
M 计秤 | 70 | ||
R 计秤 | 118 |
机械性能 | 额定值 | 单位制 | 测试方法 |
拉伸模量 | |||
-- 3 | 344000 | psi | ASTM D638 |
-- | 341000 | psi | ISO 527-2/1 |
抗张强度 | |||
屈服 4 | 8990 | psi | ASTM D638 |
屈服 | 9140 | psi | ISO 527-2/50 |
断裂 4 | 9430 | psi | ASTM D638 |
断裂 | 7250 | psi | ISO 527-2/50 |
伸长率 | |||
屈服 4 | 6.0 | % | ASTM D638 |
屈服 | 6.0 | % | ISO 527-2/50 |
断裂 4 | 120 | % | ASTM D638 |
断裂 | 70 | % | ISO 527-2/50 |
弯曲模量 | |||
1.97 in 跨距 5 | 334000 | psi | ASTM D790 |
-- 6 | 334000 | psi | ISO 178 |
弯曲强度 | |||
-- 6, 7 | 13100 | psi | ISO 178 |
屈服, 1.97 in 跨距 5 | 13500 | psi | ASTM D790 |
抗泰伯磨耗 (1000 Cycles, 1000 g, CS-17 转轮) | 10.0 | mg | ASTM D1044 |
冲击性能 | 额定值 | 单位制 | 测试方法 |
简支梁缺口冲击强度 8 | ISO 179/1eA | ||
-22°F | 4.8 | ft·lb/in2 | |
73°F | 5.7 | ft·lb/in2 | |
悬壁梁缺口冲击强度 | |||
Natural, Tints | 12 | ft·lb/in | ASTM D256 |
73°F | 12 | ft·lb/in | ASTM D256 |
-22°F 9 | 4.8 | ft·lb/in2 | ISO 180/1A |
73°F 9 | 5.7 | ft·lb/in2 | ISO 180/1A |
无缺口悬臂梁冲击 (73°F) | 60 | ft·lb/in | ASTM D4812 |
装有测量仪表的落镖冲击 (73°F, Energy at Peak Load) | 478 | in·lb | ASTM D3763 |
落锤冲击 (73°F) | 1500 | in·lb | ASTM D3029 |
拉伸冲击强度 10 | 180 | ft·lb/in2 | ASTM D1822 |
热性能 | 额定值 | 单位制 | 测试方法 |
热变形温度 | |||
66 psi, 未退火, 0.252 in | 279 | °F | ASTM D648 |
66 psi, 未退火, 3.94 in 跨距 11 | 271 | °F | ISO 75-2/Be |
264 psi, 未退火, 0.126 in | 259 | °F | ASTM D648 |
264 psi, 未退火, 0.252 in | 259 | °F | ASTM D648 |
264 psi, 未退火, 3.94 in 跨距 11 | 250 | °F | ISO 75-2/Ae |
维卡软化温度 | |||
-- | 282 | °F | ISO 306/B50 |
-- | 284 | °F | ISO 306/B120 |
Ball Pressure Test (257°F) | Pass | IEC 60695-10-2 | |
线形膨胀系数 - 流动 | |||
-40 到 203°F | 0.000038 | in/in/°F | ASTM E831 |
73 到 176°F | 0.000039 | in/in/°F | ISO 11359-2 |
比热 | 0.299 | Btu/lb/°F | ASTM C351 |
导热系数 | |||
-- | 1.3 | Btu·in/hr/ft2/°F | ASTM C177 |
-- | 1.4 | Btu·in/hr/ft2/°F | ISO 8302 |
RTI Elec | 266 | °F | UL 746 |
RTI Imp | 266 | °F | UL 746 |
RTI Str | 266 | °F | UL 746 |
电气性能 | 额定值 | 单位制 | 测试方法 |
表面电阻率 | > 1.0E+15 | ohm | IEC 60093 |
体积电阻率 | |||
-- | > 1.0E+17 | ohm·cm | ASTM D257 |
-- | > 1.0E+15 | ohm·cm | IEC 60093 |
介电强度 | |||
0.126 in, in Air | 380 | V/mil | ASTM D149 |
0.126 in, 在油中 | 430 | V/mil | IEC 60243-1 |
介电常数 | |||
50 Hz | 3.17 | ASTM D150 | |
60 Hz | 3.17 | ASTM D150 | |
1 MHz | 2.96 | ASTM D150 | |
50 Hz | 2.70 | IEC 60250 | |
60 Hz | 2.70 | IEC 60250 | |
1 MHz | 2.70 | IEC 60250 | |
耗散因数 | |||
50 Hz | 0.00090 | ASTM D150 | |
60 Hz | 0.00090 | ASTM D150 | |
1 MHz | 0.010 | ASTM D150, IEC 60250 | |
50 Hz | 0.0010 | IEC 60250 | |
60 Hz | 0.0010 | IEC 60250 | |
相比耐漏电起痕指数(CTI) | PLC 2 | UL 746 | |
高电弧燃烧指数(HAI) | PLC 1 | UL 746 | |
高电压电弧起痕速率 (HVTR) | PLC 2 | UL 746 | |
热丝引燃 (HWI) | PLC 2 | UL 746 | |
可燃性 | 额定值 | 单位制 | 测试方法 |
UL 阻燃等级 (0.0429 in) | V-2 | UL 94 | |
极限氧指数 | 25 | % | ISO 4589-2 |
光学性能 | 额定值 | 单位制 | 测试方法 |
折射率 | 1.586 | ASTM D542 | |
透射率 (100 mil) | 88.0 | % | ASTM D1003 |
雾度 (100 mil) | 1.0 | % | ASTM D1003 |
注射 | 额定值 | 单位制 | |
干燥温度 | 250 | °F | |
干燥时间 | 3.0 到 4.0 | hr | |
干燥时间,zui大 | 48 | hr | |
建议的zui大水分含量 | 0.020 | % | |
建议注入量 | 40 到 60 | % | |
螺筒后部温度 | 480 到 520 | °F | |
螺筒中部温度 | 500 到 540 | °F | |
螺筒前部温度 | 520 到 560 | °F | |
射嘴温度 | 510 到 550 | °F | |
加工(熔体)温度 | 520 到 560 | °F | |
模具温度 | 160 到 200 | °F | |
背压 | 50.0 到 100 | psi | |
螺杆转速 | 40 到 70 | rpm | |
排气孔深度 | 0.0010 到 0.0030 | in |
:何生
:86-
传真号码:86-
地址:广东 东莞市
PC基础创新塑料(南沙)HF1140-111 FDA 食品接触, 未评其它产品
PC基础创新塑料(南沙)HF1140-111 FDA 食品接触, 未评
PC基础创新塑料(南沙)HF1130R 耐热性,高
PC基础创新塑料(南沙)HF1130 耐热性,高
PC基础创新塑料(南沙)HF1130 耐热性,高
PC基础创新塑料(南沙)HF1130-111 耐热性,高
PC基础创新塑料(南沙)HF1130 WH8D312XL 电气性能与可燃性
PC基础创新塑料(南沙)HF1110R薄壁部件 镜头
PC基础创新塑料(南沙)HF1110-111薄壁部件 镜头
PC基础创新塑料(南沙) HF1110R 薄壁部件 镜头
PC基础创新塑料(南沙) HF1110R 光学数据存储